Dear Manoj,
You told in your mail that, you have 2 WPS, 5mm to 50mm ( whether this is also combined process GTAW + SMAW) ?
On Mon, Jun 6, 2011 at 5:26 PM, manoj john <manojacgnr@gmail.com> wrote:
Dear All,
I have to weld 40 mm thk ss 304 plate to be welded with root GTAW and
subsequent run by SMAW. I have 2 WPS,one WPS GTAW + SMAW thickness
range qualified is 1.6 to 12 mm and another procedure qualified 5 mm
to 50 mm with back gouging.
My doubt is can i make one wps supporting with these 2 Procedure
Root with GTAW and subsequent run with SMAW so i can carry out the
welding with GTA + SMAW 40 mm thk without further procedure
qualification.
Thanks & Regards.
Manoj
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment