Tuesday, June 7, 2011

Re: [MW:11274] Determination of Distortion based on heat input

"SYSWELD"

Thanks & Regards

K.Babu

----- Original Message -----
From: "joshi jaydeep" <jaydeep.p.joshi@gmail.com>
To: <materials-welding@googlegroups.com>
Sent: Monday, June 06, 2011 7:42 PM
Subject: [MW:11263] Determination of Distortion based on heat input


> Dear Experts,
>
> I have an issue for determining the welding distortion based on the heat
> input.
>
> Do anybody have an idea about the availability of software solution in
> market for the same.
>
> Regards,
> Jaydeep
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...