Re: [MW:11275] COMBINATION OF 2 PQR IN ONE WPS

Yes you can go head with two combine proccess wiyh one WPS. But PQR shall be qualified with WPS.

On Mon, Jun 6, 2011 at 5:26 PM, manoj john <manojacgnr@gmail.com> wrote:
Dear All,

I have to weld 40 mm thk ss 304 plate to be welded with root GTAW and
subsequent run by SMAW.  I have 2 WPS,one WPS GTAW + SMAW thickness
range qualified is 1.6 to 12 mm and another procedure qualified 5 mm
to 50 mm  with back gouging.

My doubt is  can i make one wps supporting with these 2 Procedure
Root with GTAW and subsequent run with SMAW so i can carry out the
welding with GTA + SMAW 40 mm thk without further procedure
qualification.

Thanks & Regards.
Manoj

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanking You.
 
Yours faithfully
 
For
TOLANI Projects Pvt.Ltd.
 
J.R.Parmar
09159991454
08000040871

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...