PQR should be of 3 PWHT cycle
Regards
Hegde P.b.
From: asad azmi <azmiasadayub@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sat, 4 June, 2011 5:49:30 PM
Subject: [MW:11257] simulation cycle for PQR
Dear All,
Greetings.
A Vessel of CS MATERIAL, 10 thk, is having Simulation ( 3 Cycles PWHT) requirement. PWHT soaking time for the vessel is 2 hours.PWHT is Service Requirement.
construction code - ASME sec VIII Div 1.
Whether PQR Should have 3 Cycles PWHT or Single cycle PWHT only.
Thanks and Regards
Asad Azmi
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.