Sunday, June 5, 2011

[MW:11260] Re: simulation cycle for PQR

dear azmi,

better if u have 3 cycled qualified PQR.this will cover your post PWHT
repair if any arise after NDE(RT).


On Jun 4, 1:19 pm, asad azmi <azmiasada...@gmail.com> wrote:
> Dear All,
>
> Greetings.
>
> A Vessel  of CS MATERIAL, 10 thk, is  having Simulation ( 3 Cycles PWHT)
> requirement. PWHT soaking time for the vessel is  2 hours.PWHT is Service
>  Requirement.
>
> construction code - ASME sec VIII Div 1.
>
> Whether PQR Should have  3 Cycles PWHT or Single cycle PWHT only.
>
> Thanks and Regards
>
> Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...