Tuesday, June 7, 2011

[MW:11278] thickness limitation for a WPS

Dear Experts

What will be the thickness limitation when a WPS is qualified with a
PWHT above the upper transformation temperature.
For example : Material 12 MM THICK SA516 GR.70 WELDED BY GTAW+SMAW AND
PWHT DONE AT 900 DEG. C
with and with out Impact requirement.


--
Regards
Ajay Singh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...