Wednesday, February 16, 2011

Re: [MW:9906] RT film interpretation as per B31.3

Dear Sebastian


Elongated void can happens between the weld bead and the surface of side wall in the root.

 

B31.3 does not say detail of BT. If you can not get the acceptance criteria in your project specification, the issuance of a TQ (technical query) is more advisable.

 

If the density exceeds the parent material, it confirms that root surface concave is slightly below the material.

 

Let this helps you



2011/2/16 sebastin wilson <asswilson@gmail.com>


---------- Forwarded message ----------
From: sebastin wilson <asswilson@gmail.com>
Date: Tue, Feb 15, 2011 at 9:19 PM
Subject: Re: [MW:9768] welding machine qualificatio
To: materials-welding@googlegroups.com


Dear All

According to B31.3, Please clarify the following which will helpful for RT film interpretation.
a.Can lack of fusion occur in root pass?  My opinion B31.3 341.3.2.sketch is only given as examples. I understood from the picture (C) LF will be consider as IP in that particular case other case like if no HI-LO will be consider as Lack of fusion(If one root edge is not fused).
B.Acceptance critria as per B31.3 for Burn through(BT).I cannot find the relevant details from code book.
C.Acceptance critria as per B31.3, how we measure root concavity by RT if no access? Is densitometer allowed to perform?
I am waiting for your answer on this subject.
With kind regards

A.S.Wilson




On Mon, Feb 7, 2011 at 9:07 PM, <TRavikumar@flowserve.com> wrote:
 Dear all

 In welder qualification and new  process establisment  as per sec ix  . weld consumabels ,test coupons &weldrs are our only using the welding m/c from the subsuplliers place is it valid for qualification .since the welding machine is not  variabel


RAVIKUMAR T S
SENIOR ENGINEER-
FLOWSERVE INDIA CONTROLS PVT.LTD
PLOT#4,1A,EPIP WHITWFIELD
BANGALORE-560066,INDIA
PHONE:91-8028410289-90
FAX       :91-8028410286
E-MAIL :travikumar@flowserve.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...