Re: [MW:9371] Will fillet welder qualified to tack the groove Joint

Yes, u can use fillet welder for tacking purpose becouse there is no tack welder qualification in ASME
Regards
Moorthy


From: Kathalingam Babu <kathalingam.qaqc@ppl.com.sg>
To: materials-welding@googlegroups.com
Sent: Fri, January 21, 2011 12:15:16 PM
Subject: [MW:9365] Will fillet welder qualified to tack the groove Joint

Hi all
 
Any one share official interpretation for the below situation.
 
Will the ASME fillet welder ,qualified to tack weld the  groove joint in fitup ?
 
Thanks & Regards,
 
K. Babu

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...