Hi, You haven't mention the Speciment thickness,so cant tell you the no.of test specimen required. You can refer with QW451.1 for the test specimen and no.of tests required according to thickness. Thanks & Regards, (Karthik) Karthikeyan.S QA/QC Manager Getabec Energy Co.,Ltd. 379,Moo6,Soi8,Nikhomphatana, Rayong-21180, Thailand. Phone: 0066 38 897035-8 (Off) Fax: 0066 38 897034 Hand Phone: 0066 892512282 --- On Tue, 1/18/11, siva prasad <siva_chinnam@yahoo.co.in> wrote:
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.