Dear Martin,

                                If you have ASME assigned you can use ASME VIII Appendix R

                                If you have AWS D1.1 listed material you can use AWS D1.1 table 4.9 or  Annex I guideline on alternative method for determining preheat

 

Or you can use the following formula for fast calculations.

 

 

Best regards, 

Yassein Abdou

Welding & Grating Manager

energya STEEL FABRICATION 

 

 

 

 

 

 


Egypt Factory & Head Office: Industrial Zone A 6 East, 10th of Ramadan City

Tel         +2015 412 239 - 412 249 / +2010 002 0133

Fax        +2015 412 236

Cairo Office: 98 a Hassan Mamoun St. Naser City, Cairo Egypt

Tel         +2 02 22706306 - 2714 631 Fax +2 02 22752 701

KSA Factory: Rabigh - Yanbu High Way Exit 927 Industrial Zone Aramco Road. 

Tel:          +966 500 150 706 Fax : +966 500 592

Jeddah Office: Haifa Building. King Road  Jeddah City, Saudi Arabia

Tel         +966 2 2907382  Fax +966 2 6882901

www.energyasteel.com           info@energyasteel.com

Personal Mobile: + 2010 0400361     email: yassein.abdou@energyasteel.com

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Martin Prad
Sent: 13 January, 2011 9:01 AM


To: materials-welding@googlegroups.com
Subject: [MW:9205] preheat calculation

 

Hi freinds,
 
How to calculate a preheat? Is the any mathematic formula for this?
 
kind regards,
 
Martin.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
அருணாசலம்
கலைவாணி
சுதர்ஷனா
வருண்


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35001] Cold pass

Dear Rithvik, In duplex stainless steel (DSS) or super duplex stainless steel (SDSS) welding, the terms "hot pass" and "cold ...