Please provide the PWHT requirement for the Pipe to Weldolet joint.
 
 
Main Run Pipe material    : API 5L Gr.B- PSL2
 
Run Pipe Size                    : 20 inch, Sch : 100 ( Thick : 32.54 mm)
 
Branch connection            : Weldolet ( 20 x 6 inch , Sch : 120 )
 
Weldolet material            :  A 105.
 
Weldolet attachment       : as per Fig : 328.5.4 D- Sketch 1 of ASME B 31.3
 
Reference standard        : ASME B -31.3 & NACE MR-0175.
 
 
 
As the welding  shall meet the requirements as per NACE MR 0175, whether can we waive the PWHT requirements for the pipe to  branch weld, if the hardness value is less than 22 HRC.
 
 
 
 
Regards
 