Thursday, November 18, 2010

Re: [MW:8309] welder qualification for ASME U stamp vessel

Hi,

Welder qualification is a manufacturer's responsibility as per the code specification/requirements.Welder qualification records shall be reviewed by AI.

No need to witness by third party unless otherwise the customer's requirement.



Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 11/17/10, Santosh Gaikwad <santoshcwi@gmail.com> wrote:

From: Santosh Gaikwad <santoshcwi@gmail.com>
Subject: [MW:8304] welder qualification for ASME U stamp vessel
To: materials-welding@googlegroups.com
Date: Wednesday, November 17, 2010, 7:37 PM

Dear all,
could you please give information regarding welder qualification,i am trying to qualify some new welder for ASME U stamp vessel ,do i need to call third party inspection agency for witness or just i go ahead & run the welder qualification test & get welder certificate endorsed  from AI.

kind regards

Santosh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...