Hi Baiju
There is no welding process for GRP. The joint is made by overlay of laminate.ie by reinforcing resin with fiberglass mat. Refer BS 4994 or ASME section X for further reading.

Regards
Hrishi
Sent on my BlackBerry® from Vodafone

-----Original Message-----
From: Baiju nair <nairbaiju@ymail.com>
Sender: materials-welding@googlegroups.com
Date: Mon, 1 Nov 2010 09:14:57
To: Materials & Welding<materials-welding@googlegroups.com>
Reply-To: materials-welding@googlegroups.com
Subject: [MW:0] grp welding process

Dear Sir,

I want to know about grp welding process.

with Regards,
Baiju s nair.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...