[MW:8112] E7018 & E7018-1

Hi everybody

What is meaning of " -1 " in electrode E7018-1
Is it indicate hydrogen diffusion

What is the difference between E7018 & E7018-1, only impact test or
material composition also


Reg

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.