Re: Re: [MW:7388] Electrode for cast steel


Magna 303 Gold an option for critical repair job. Suitable for any family of steel.

Regards

VISHAL MEHTA

SUPERTECH SERVICES LTD

Sent on my BlackBerry® from Vodafone


From: "venkadakumar " <venkadakumar@rediffmail.com>
Sender: materials-welding@googlegroups.com
Date: 5 Oct 2010 16:46:51 -0000
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: Re: Re: [MW:7381] Electrode for cast steel



Hi,

Best choice is UTP 65,German Make or Eutectic+ castolin 680 or 680 CGS
Both electrodes you can weld any unknown steel without making severe investigation about Base materail.

Regards

Venkat

On Sun, 03 Oct 2010 14:27:19 +0530 wrote
>There are several electrodes for this, they are based in Nickel, so even you can use a Stainless electrode. Regards.
>
>
2010/9/30 Larry <quality@unieng.com.au>
>

Hi,

 

Can anybody suggest a good electrode for cast steel?

 

No code applies, just common welding.

 

 

Thanks in advance.

 

 

 

Cheers,

Larry

--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

>

--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...