Monday, October 25, 2010

Re: [MW:7786] MW: 7740- Requirements for welding of A517-Gr.B

Dear Pradip,

Thanks for your help, but now, I want to know, is there any requirement to use postheating or slow cooling down by a heat resistant blanket such as asbestos

after welding of A517 steel?

 
Thanks.
Kianoush Zarrin naghsh.

--- On Sun, 10/24/10, pgoswami <pgoswami@quickclic.net> wrote:

From: pgoswami <pgoswami@quickclic.net>
Subject: [MW:7776] MW: 7740- Requirements for welding of A517-Gr.B
To: materials-welding@googlegroups.com
Date: Sunday, October 24, 2010, 3:27 PM

Hi Kianoush,
 
Attached are some guidelines  on A/SA-517 steel. This steel is a Q&T steel contains various alloying elements (different grades have different compositions). Welding of this steel would require a precise control of heat input and welding parameters and correct selection of welding electrodes.
 
Generally there's no electrodes of exact matching chemistry for this steel. However if I have to make a choice , the preference would be either E-9018/10018/11018M SMAW electrodes and matching GTAW, GMAW  and SAW filer depending on the process and  extent of fabrication involved.
 
Many fabricators may prefer E-9018/10018/11018G (General Low Alloy Steel) electrodes, but if the desired chemistry is specified beforehand, so that there would not be any later surprises?
 
What's the design code ? For fabricating A-517 steel one has to incorporate strictly the design code requirements.
 
Let me know if the attached information helps you or not?.
 
Thanks.
 
Pradip Goswami,P.Eng.
Welding & Metallurgical Specialist & Consultant
Email-pgoswami@sympatico.ca,
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of kianoosh zarrin naghsh
Sent: Saturday, October 23, 2010 10:10 AM
To: materials-welding@googlegroups.com
Subject: [MW:7740] Requirements for welding of A517-Gr.B

Dear All,
Is there any experience on welding of A517-Gr.B with thickness up to 20 mm?
 
Thanks,
Kianoush Zarrin naghsh

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...