Monday, October 25, 2010

Re: [MW:7774] ASME BPV SEC IX Material Range issue

Dear Limesh,
 
My interpretation with QW-403.5 as Below.
 

1. Is there any problem for welding P1 Group No.1 to P1 Group No.1  &  P1 Group No.2 to P1 Group No.2 based on above PQR?

You Cannot write WPS for the above combinations with existing PQR.

.2.Can I write separate WPS (with impact test) based on above PQR for,

Material – P1 Group No. 1 to P1 Group No. 1

Material – P2 Group No. 2 to P2 Group No. 2

 
However, if you have the PQR Qualifications for the P1 Group No. 1 to P1 Group No. 1 & P1 Group No. 2 to P1 Group No. 2 combinations with same essential, non-essential variables,
 
Then you can write the WPS for  the P1G1 to P1 G2 , with qualifying P1G1 to P1G2  materials.
 
 
Thanks & Regards
 
K.Babu
Singapore
 
 
 
----- Original Message -----
From: limesh M
Sent: Sunday, October 24, 2010 10:42 PM
Subject: [MW:7767] ASME BPV SEC IX Material Range issue

Dear All,

 

I need your help in the following subject.
 

Design Code – ASME B31.3

Welding Code – ASME BPV SECTION IX

I have a PQR for the following material classification as per ASME BPV SEC IX

Material – P1 Group No. 1 to P1 Group No. 2

Weld Metal Impact Tested – Yes

 

My query is that,

1. Is there any problem for welding P1 Group No.1 to P1 Group No.1  &  P1 Group No.2 to P1 Group No.2 based on above PQR?

2.  Can I write separate WPS (with impact test) based on above PQR for,

Material – P1 Group No. 1 to P1 Group No. 1

Material – P2 Group No. 2 to P2 Group No. 2

 

My next query is that,

Is there any problem for showing all material range in a single WPS based on above PQR?

Ie, qualified range of materials- P1 Group No. 1 & P1 Group No. 2 in the same WPS.
 
 
Regards,
 
Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...