Monday, October 25, 2010

Re: [MW:7772] Unlisted Materials welding AWS D1.1

Aneesh,
 
Cl:4.7 discuss about the WPS not the WQT.
 
Check the table 4.11, which says, material group is non-essential variable as per AWS D1.1.
 
Regards
 
K.Babu
Singapore
 
----- Original Message -----
Sent: Sunday, October 24, 2010 11:06 AM
Subject: Re: [MW:7752] Unlisted Materials welding AWS D1.1

how do i get the free qualified welder i can use the wqt?


From: aneesh <aneeshgopikc@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Saturday, October 23, 2010 8:10:17 PM
Subject: [MW:7734] Unlisted Materials welding AWS D1.1


1. Can we do the unlisted materials( EN materials) welding by a
welder who qualified in Group 2 material as per AWS D1.1?
2. The D1.1 says unlisted materials shall be qualified by Qualifcation
( point 4.7 D1.1 2004) so  we can't use prequalified WPSs for unlisted
materials, write?

Please advice...

Regards,
Aneesh
KSA

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...