Re: [MW:7754] European code for Preparing&Qualifying WPS(Piping)

Dear Limesh

 

EN ISO 15609-1:2004 supersedes EN 288-2:1992

G.S.Arora
Ph: 91-9725262404


--- On Sat, 23/10/10, Clubb, Archie <Archie.Clubb@veoliawater.com> wrote:

From: Clubb, Archie <Archie.Clubb@veoliawater.com>
Subject: Re: [MW:7748] European code for Preparing&Qualifying WPS(Piping)
To: materials-welding@googlegroups.com
Date: Saturday, 23 October, 2010, 10:09 PM

One procedure one performance - and more onerous than ASME! Check new numbers!


From: materials-welding@googlegroups.com <materials-welding@googlegroups.com>
To: materials-welding@googlegroups.com <materials-welding@googlegroups.com>
Sent: Sat Oct 23 15:54:13 2010
Subject: Re: [MW:7741] European code for Preparing&Qualifying WPS(Piping)

Dear All,
 
Then what is this BS EN ISO15609 & BS EN ISO15614-1 ?What is the relation between BS EN 288&287 with BS EN ISO 15609-1 &BS EN ISO 15614-1.I found somewhere that EN 287 is for welder qualification !!! I am totally confused.
 
Regards,
 
Limesh

On Sat, Oct 23, 2010 at 5:08 PM, Clubb, Archie <Archie.Clubb@veoliawater.com> wrote:
BS EN 288 & 287

A


From: materials-welding@googlegroups.com <materials-welding@googlegroups.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Sat Oct 23 05:21:50 2010
Subject: [MW:7728] European code for Preparing&Qualifying WPS(Piping)

Dear All,
 
What is the european code(s) for preparing and qualifying welding procedure specification for process piping.
 
 
Regards,
 
Limesh
 
 
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
************************************************************************* This e-mail message and any attachments to it are intended only for the  named recipients and may contain confidential information. If you are not one of the intended recipients, please do not duplicate or forward this e-mail message and immediately delete it from your computer. If you  received this email in error, please notify postmaster@veoliawater.com *************************************************************************       
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
************************************************************************* This e-mail message and any attachments to it are intended only for the  named recipients and may contain confidential information. If you are not one of the intended recipients, please do not duplicate or forward this e-mail message and immediately delete it from your computer. If you  received this email in error, please notify postmaster@veoliawater.com *************************************************************************       
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...