Dear friend,
Yes, U can. but you have to qualified as mentioned WPS parameters.
 
regards
Sujay


 
On Thu, Oct 21, 2010 at 11:26 AM, Engineer Mech <mengineer010@gmail.com> wrote:
Dear all

I have to qualify welders, we r having qualified WPSs of our sister
concern co,
Can i go directly to WQT only with tat wpss With TPI,
Is it possible, pl let me know..

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...