Thursday, October 21, 2010

Re: [MW:7686] Regarding Seam in Piping

ASME B 31.3 has no restriction on such type of longitudinal welds in the same plane. In your case seam staggering is not possible.

FYI, ASME Sec VIII Div I - UW 9 (d) allows this type of situation with radiography of at the intersection with 100 mm length minimum on both side from the center. 

You may propose case accordingly to your client for final acceptance.

Regds/Jignesh

On Thu, Oct 21, 2010 at 11:37 AM, amman <ammankhan77@gmail.com> wrote:
Dear All,

I Want to know that seam to seam is not allowed during fit-up or
welding of Piping as per 31.3
but today i had observed 16" A312 SCH10S same elbow to elbow fit-up in
up direction we have to done fit-up but it comes seam to seam other
way is not possible.

can u suggest me regarding this issue.

Shaikh Ahmed
QA/QC engineer.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...