Re: [MW:7636] Change in electrode manufacturer

Hi,
You can use.The brand is a non essential variable.
 
Thanks & Regards,
 
(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 10/19/10, krishna <wiqw@rediffmail.com> wrote:

From: krishna <wiqw@rediffmail.com>
Subject: [MW:7635] Change in electrode manufacturer
To: materials-welding@googlegroups.com
Date: Tuesday, October 19, 2010, 11:15 AM

Hi frnds,
Please clarify the below

we have qualified a welding procedure with ESAB E07018 and it is passed we are doing the production welding .

Now we have no stock of ESAB so we are using HONAVAR Electrodes with the same WPS.

Is it acceptable or we have to make another procedure with honavar electordes.

regards,
kk
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...