RE: [MW:7617] Normalizing of Weld joints

Impact value will increase.

 

Regards

M.G.Kattimani

 

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of GANESH GANESH
Sent:
Sunday, October 17, 2010 9:02 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:7615] Normalizing of Weld joints

 

whether impact value after normalizing of weld joint decrease or increase

 


From: Vanchinath S.A. <vanchinaths@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sun, 17 October, 2010 4:38:35 PM
Subject: Re: [MW:7611] Normalizing of Weld joints

normalising temp should be in the range of 880 to 920 degC and soaking time 1/2 hr per inch thk. higher soaking time will result in lowering of weld strength.

vanchi

On Sat, Oct 16, 2010 at 5:40 PM, pavainathan <pavainathan@gmail.com> wrote:

Hi Memebers,
                     We have welded fitting (A 234 WPBW) which needs
to be Normalized after welding around temeperature 825 DegC .I look
for some specification reference to calculate the soaking time for the
thickness range 20-25mm . Any one can suggest me the options.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...