normalising temp should be in the range of 880 to 920 degC and soaking time 1/2 hr per inch thk. higher soaking time will result in lowering of weld strength.
vanchi

On Sat, Oct 16, 2010 at 5:40 PM, pavainathan <pavainathan@gmail.com> wrote:
Hi Memebers,
                     We have welded fitting (A 234 WPBW) which needs
to be Normalized after welding around temeperature 825 DegC .I look
for some specification reference to calculate the soaking time for the
thickness range 20-25mm . Any one can suggest me the options.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...