Thursday, October 14, 2010

Re: [MW:7558] EN10204 3.2 certification

Hi,
3.2 is a inspection document for metallic materials not for pressure vessels.Pressure vessels shall be certified with the manufacturer's data report by the manufacturer along with the suppported inspection reports/documents.(for example Form U1/U1A....for pressure vessel constructed by ASME Section VIII,Div.1)
 
Thanks & Regards,
 
(karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Thu, 10/14/10, limesh M <limesh78@gmail.com> wrote:

From: limesh M <limesh78@gmail.com>
Subject: Re: [MW:7554] EN10204 3.2 certification
To: materials-welding@googlegroups.com
Date: Thursday, October 14, 2010, 3:20 PM

Dear Aarpee,
 
I don't know how to interpret,but one thing I can say,3.2 certification is applicable to valves based on customer requirement(In our current project we are purchasing valves with 3.2 certificates).3.2 certification on Pressure vessels,hmmm,I don't know.Seniors advise is required.
 
 
Regards,
 
Limesh

On Thu, Oct 14, 2010 at 10:58 AM, Aarpee <ramprasad.chari@gmail.com> wrote:
Dear all,
Can 3.2 certfication be applied to Valves and Pressure vessels OR can
3.2 certification be applied to "assembled' and "welded" products?
This query is due to scope defined in the standard as:
"This document specifies different types of inspection documents
supplied to the purchaser in accordance with the requirements of the
order,for delivery of all metallic products e.g
plates,sheets,bars,forgings,castings,whatever their method of
production"

I wish to have your views/interpretation/experience on above.

Regards
Aarpee

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.