Thursday, October 14, 2010

RE: [MW:7557] GMAW instead of GTAW +SMAW

All

 

Agree with Karthic – the use of GMAW and FCAW are simply to speed up and cheapen the work ! – Bang goes the quality – Stick to the TIG as far as possible at roots.

 

 

 

Archie

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of hany alfy
Sent: 14 October 2010 06:26
To: materials-welding@googlegroups.com
Subject: Re: [MW:7547] GMAW instead of GTAW +SMAW

 

You can use GMAW no problems

Use Metalloy Wires it is give good reuslts with the proper WPS/PQR

for CS Pipes u can use Metalloy 76 i attached the data for you here (Before it was Metalloy 71)

if u need any more pls contact me

Hani Alfe

 


From: Karthik <karthik6684@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Thu, October 14, 2010 8:08:22 AM
Subject: Re: [MW:7544] GMAW instead of GTAW +SMAW


Hi,

Normally GMAW is not allowed in piping and pressure vessel welding because of the more weld defects even which cannot identify in RT.

But With proper application and appropriate parameters, excellent welds can be produced using short-circuit GMAW.  However, if the welder is not careful to follow established procedures, a number of serious weld defects can occur.

The most significant of these defects is lack of sidewall fusion; the molten puddle of metal does not fully fuse with the pipe sidewalls, and a "cold lap" defect occurs.  This is a significant structural defect that is difficult to identify with commonly used nondestructive inspection methods such as radiography.  So while the GMAW and FCAW processes have gained popularity for many applications, they have not been considered serious options for most pipe welding operations.

This poor reputation is no longer deserved, however.  Continuous development in both power supply and consumable technology have made this process a viable alternative to manual GTAW or shielded metal arc welding (SMAW) of pipe.

Thanks & Regards,

 

(Karthik)

Karthikeyan.S

QA/QC Manager

Getabec Energy Co.,Ltd.

379,Moo6,Soi8,Nikhomphatana,

Rayong-21180,

Thailand.

Phone: 0066 38 897035-8 (Off)

Fax: 0066 38 897034

Hand Phone: 0066 892512282



--- On Thu, 10/14/10, rupeshjambhale@gmail.com <rupeshjambhale@gmail.com> wrote:


From: rupeshjambhale@gmail.com <rupeshjambhale@gmail.com>
Subject: [MW:7543] GMAW instead of GTAW +SMAW
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Thursday, October 14, 2010, 10:50 AM

Our contractor want to use GMAW process inplace of GTAW+SMAW
for cS pipe butt weld joint. Construction code is B31.3  . Can we quaLify OR use GMAW  inplace of Gtaw+ smaw process. Pressure is 15 kg/cm2g with full RT. Pls advice?bscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



     

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

***************************************************************************************************************************************************************************
This e-mail (which includes any files attached to it), it is intended solely for the named recipient and may contain CONFIDENTIAL, legally privileged or trade
secret information protected by law. It has been sent it via the internet and is therefore not secure against corruption, interception or unauthorised modification.

If you are not the intended recipient please do not read, use, disclose, distribute, copy, print or rely on any information contained in this e-mail. Please
immediately notify us by telephoning +44 (0) 1494 887808 or return it to us by e-mail to the sender, confirming that this e-mail has been deleted from
your system and any hard copies destroyed.

To the extent permitted by law, neither we nor any of our subsidiaries, parent entities or other affiliates, nor any employee, director or officer thereof,
accepts any liability whatsoever in relation to this e-mail including liability arising from any external breach of security or confidentiality or for virus
infection or for statements made which are clearly the sender's own and not made on our behalf.

"We" and "our" in this footer refer to the following legal entity:

VWS Westgarth Ltd. Registered in Scotland No. 147604, Orbital House, 3 Redwood Crescent, East Kilbride, G74 5PR

This company is a member of the Veolia Water Solutions & Technologies group, but please contact the sender should you have any question
regarding the legal entity on whose behalf this email was sent.
***************************************************************************************************************************************************************************

 ************************************************************************* This e-mail message and any attachments to it are intended only for the  named recipients and may contain confidential information. If you are not one of the intended recipients, please do not duplicate or forward this e-mail message and immediately delete it from your computer. If you  received this email in error, please notify postmaster@veoliawater.com *************************************************************************       

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...