Re: [MW:7549] Difference between 100% RADIOGRAPHY & Full RADIOGRAPHY

Check UW 11 Cl 4.0 under "full radiography" in ASME Section VIII Div 1
100% radiography means ALL BUTT WELDED joints
Regards
Aarpee

On Wed, Oct 13, 2010 at 10:56 AM, hemant solanki <h_solanki@rediffmail.com> wrote:

Dear All,

Could you please tell me what is the difference between 100% radiography & fully radiography? Is it clarified in ASME code?

Thanks,
Hemant Solanki


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...