Yes correct.
 
EN 10025-2, Gr S275JR is equivalent to ASTM A36
 
Rgds
 
Babu
 
----- Original Message -----
From: limesh M
Sent: Tuesday, October 12, 2010 10:22 PM
Subject: [MW:7508] Material Equivalent

Dear All,
 
I need your help.Is it true that ASTM A36 is equivalent to BSEN 10025-2 Gr.S275JR? Is there any other material equivalent to BSEN 10025-2Gr.275JR? I am looking for ASTM equivalents.
 
 
Regards,
 
Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...