Dear Mr. Suresh,
                          For radiography of WQT min. 150mm weld length is required.

2010/10/12 suresh kochayatu <sureshkochayatu@gmail.com>
Dear gents,
could any body help me regarding following issues,
1, Can we use 2 welders for WQT, for a 4" dia pipe test coupon if yes
,then what is the minimum size  limit for the combined WQT,
2,  Can I use less than 100mm test coupon  (PIPE) for WQT, which have
only visual and R.T
Thanks and regards,
Suresh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...