Friday, October 8, 2010

Re: [MW:7441] Why IGC Samples of PQRs fail?

It is important how the sample for IGC test is taken There should not be contamination of base metal or even 309 chemistry

Sent from my BlackBerry® smartphone from !DEA


From: jignesh makwana <jkmakwana5@gmail.com>
Sender: materials-welding@googlegroups.com
Date: Thu, 7 Oct 2010 17:29:54 +0530
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: [MW:7437] Why IGC Samples of PQRs fail?

Dear All, Dear Jeff, Please look into.
Please find the attachment
All the PQRs have been failed except one sr. no. 4 in IGC testing as ASTM A 262 Practice E.
Can anybody suggest me any solution or any reason??
Preheating @ 100 C
Interpass @ 150 C

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...