This is available in API 570 under definitions of test point as given below:
 
Quote:
 

3.46 test point:

An area defined by a circle having a diameter

not greater than 2 inches (50 mm) for a line diameter not

exceeding 10 inches (250 mm), or not greater than 3 inches

(75 mm) for larger lines. Thickness readings may be averaged

within this area. A test point shall be within a thickness measurement location.

 

Regards,



On Wed, Oct 6, 2010 at 10:31 AM, M. Ali <mali5286@gmail.com> wrote:
Dear All,

TML or Thickness Measurement Locations are marked on piping for
inference of corrosion rates and inspection intervals. I have been
reading API 570 and API 574 to determine the recommended size of a TML
according to cade but cannot find it.
Can anybody please indicate?


Thanks and Regards,

Muhammad Ali

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...