RE: [MW:7385] Unable to find Oven Baking Temp in ASME SEC 2 C for E309 L - 15

Not correct – stainless steel SMAW electrodes  -15, -16, -17 are low hydrogen electrodes and are hygroscopic.  Once the hermetically sealed containers are opened, the electrodes must be stored in an oven like other electrodes.  While 300 series materials are resistant to hydrogen assisted cracking, inadequately dried electrodes can result in weld metal porosity.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Engineering Solution
Sent: Tuesday, October 05, 2010 8:38 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:7378] Unable to find Oven Baking Temp in ASME SEC 2 C for E309 L - 15

 

Dear all

no need backing for SS electrode or any 30 series but you should have to make sure that electrode should be moisture less.

 

regards - babar



 

On Tue, Oct 5, 2010 at 5:59 AM, arvinda shan <arvindashan@gmail.com> wrote:

Dear Hegde,

 

You can see all electrodes pockets they marked baking temperature and duration. Sec II c also refered manufacturer recommendations.

 

arvinda.

On Mon, Oct 4, 2010 at 7:57 PM, <hegde.pb@isgec.com> wrote:

Generaly SS. Electrodes are recomended to bake at 250 c for 1.5 to 2 hrs and hold at 100. C till being issued to welder . Higher baking temp. Say 300 c causes problm of peelng of flux coatinhg
Regards
Hegde

Sent from my BlackBerry® smartphone from !DEA


From: arvinda shan <arvindashan@gmail.com>

Date: Mon, 4 Oct 2010 17:47:36 +0400

Subject: Re: [MW:7359] Unable to find Oven Baking Temp in ASME SEC 2 C for E 309 L - 15

 

manufacturer recommendation baking temperature to be followed.

 

arvinda.

On Mon, Oct 4, 2010 at 4:57 PM, Engineer Mech <mengineer010@gmail.com> wrote:

Dear All

I want to know baking temp of E 309 L - 15,
I checked out in SFA 5.4 in ASME sec 2 C,
Pl let me.. wat it is?

Thanks

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--

To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--

To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--

To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...