[MW:7771] Metal cored wire for SAW

Hello friends,

 

I want to know the source for alloy steel metal cored wire in 2.5/3.15/4  mm  (eq. to EB-2 or 3) for SAW process.

Can anybody tell me.

 

Regards

Ravinder

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Arun Das
Sent: Sunday, October 24, 2010 6:06 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:7766] coating or painting

 

Dear mr.Rao,

 

Normally the pipe lines are buried in soil, hence the thickness of the protective layer,coating/painting, should be considerd and, also various mechanical properties, such as permeability of water, ability to withstand pressure due to soil expansion/contraction as the climate changes, bacterial attack resistace etc etc. Normally life span of the pipe line is considered as 75 years during the design, so we have select the option matching that too.

Hope you know that recoating is not viable on undergroud pipelines. so various aspects are there.

Painting above ground considerations include decorative aspects and protective aspects. Also economical considerations will be there.

 

Hope you got the point.

 

Thanks and regards,
 

Arun S Das

Inspection Engineer

Velosi Certification LLC

Qatar

Mob: +97433240549

+919847051202 ( India )

 

 


From: srinivas rao <ksrvasu@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sun, 24 October, 2010 3:04:19 PM
Subject: [MW:7759] coating or painting

Dear All,

Why is coating preferred in pipelines but not painting and painting but not coating in AG piping? why not vice-versa? Is it that corrosion is more due to earth?

regards,
srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...