[MW:7734] Unlisted Materials welding AWS D1.1

1. Can we do the unlisted materials( EN materials) welding by a
welder who qualified in Group 2 material as per AWS D1.1?
2. The D1.1 says unlisted materials shall be qualified by Qualifcation
( point 4.7 D1.1 2004) so we can't use prequalified WPSs for unlisted
materials, write?

Please advice...

Regards,
Aneesh
KSA

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...