Wednesday, October 20, 2010

[MW:7663] RE: 7650] ASEM equivalent of EN 1025 S355JR

 

ASTM equivalent of EN 10025-2-S355JR  is ASTM A572 GR.50

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Paul Osikwemhe
Sent: Tuesday, October 19, 2010 3:16 PM
To: materials-welding@googlegroups.com
Subject: [MW:7650] ASEM equivalent of EN 1025 S355JR

 

Dear all, can some help me with ASEM equivalent of EN 10025-2-S355JR

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...