Hi

It can do with respect to UG 10 of Sec. VIII Div.1 as guidance.

Regards

S.T.RAJAPPAN

Sr.QA/QC Engineer

cid:image001.jpg@01C9AA3F.494B1A10

Mob: +971 50 8126147

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Aly
Sent: Monday, October 18, 2010 7:33 AM
To: materials-welding@googlegroups.com
Subject: [MW:7620] Re certification of ASTM A283 GrC plate to ASTM A36

 

Dear All,

Please provide your valuable suggestion for following:

 

Can we recertify ASTM A283 Gr C plate to ASTM A36 grade?

 

Thanks for cooperation

 

Mhaskar Aly

FREE Animations for your email - by IncrediMail! Click Here!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...