Wednesday, October 13, 2010

[MW:7532] Expanding Alloy 20 Tubes


We are going to use Alloy 20 tubes in a heat exchanger,we will expand approx 200 mm length into grooves and then seal weld.
We have been told expansion is difficult, has anyone had any experience of this procedure.

John Hardcastle
 
Fabrication Manager

Euro Mechanical Contractors Company Factory
P.O. Box 46153
Abu Dhabi
United Arab Emirates
 
Phone: +971 2 550 08 99
Fax: +971 2 5501898
Mobile: +971 50 4445873
 
Email: jhardcastle@euromechanical.com
www.euromechanical.com



This email is intended for the addressee(s) only, and may contain confidential or privileged information. Unauthorised use of this information, or distribution, copying or other dissemination is strictly prohibited.

If you have received this email in error, please destroy it immediately.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...