[MW:7453] Re: EN & ASME equivalent

Dear Karthik,

The document you send regarding equivalents between ASME and EN
materials is not an comparison of materials but a technical
recommendation which provides group no.'s for WPS / PQR qualification
when qualifying according to EN specifications.

Best Regards,

Herman Pieper

On 8 okt, 07:34, Karthik <karthik6...@yahoo.com> wrote:
> Hi,
> Pls.find the attachment for EN and ASME comparison
>  
> Thanks & Regards,
>  
> (Karthik)
>
> Karthikeyan.S
> QA/QC Manager
> Getabec Energy Co.,Ltd.
> 379,Moo6,Soi8,Nikhomphatana,
> Rayong-21180,
> Thailand.
> Phone: 0066 38 897035-8 (Off)
> Fax: 0066 38 897034
> Hand Phone: 0066 892512282
>
> --- On Fri, 10/8/10, Eng/ Mostafa Kamel Hussein <mkh_...@yahoo.com> wrote:
>
> From: Eng/ Mostafa Kamel Hussein <mkh_...@yahoo.com>
> Subject: [MW:7439] EN & ASME equivalent
> To: materials-welding@googlegroups.com
> Date: Friday, October 8, 2010, 10:23 AM
>
> Dear sir,
>
> Iam material inspector and i need paper including the equivalent between the EN and ASME materials
>
> Regards, 
>
> SaSa
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
>  iso-tr20173_2006-09.pdf(Material EN Compare to ASME,ASTM).pdf
> 879KWeergevenDownloaden

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...