[MW:7445] ASME sec 9 (QW 452 & 351) doubt

Dear all,
               I came across the interpretation of Sec 9 issued by ASME on year 1988. The question was

            A performance qualification groove weld test coupon has been successfully made by a welder on a  ¾ " thick test coupon using transverse bend tests in accordance with QW-452. The test weld was made with one process, utilizing filler metals of two different F-numbers. Is the deposited weld metal thickness qualified, for each of the F-number filler metals used in qualification, "max . to be welded". (Interpretation: IX-89-02  issued date OCT 6, 1988)

The answer given by the committee is YES .

Anybody agreeing with this answer?If yes please give the relevant statements in ASME sec 9 supporting that. 

Is this answer true if interpretation is as per ASME sec 9 2007 Ed ?


--
- Sreejith -

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...