[MW:7437] Why IGC Samples of PQRs fail?

Dear All, Dear Jeff, Please look into.
Please find the attachment
All the PQRs have been failed except one sr. no. 4 in IGC testing as ASTM A 262 Practice E.
Can anybody suggest me any solution or any reason??
Preheating @ 100 C
Interpass @ 150 C

--