Wednesday, September 29, 2010

Re: [MW:7270] COKE DRUM PNEUMATIC TEST

Please specify the code/ standard to which the coke drum is built and refer whehter it is allowed / acceptable as per the code. For e.g: as per ASME Sec.VIII Div.1 it is acceptable, please refer UG-100.
 
Dokku Ajay Kumar
Mobile: +966 500071054



From: "Kavathekar, Sachin" <Sachin.Kavathekar@jacobs.com>
To: materials-welding@googlegroups.com
Sent: Tue, September 28, 2010 1:49:29 PM
Subject: [MW:7247] COKE DRUM PNEUMATIC TEST



Hi all,

My vendor has raised concession request regarding pneumatic test instead of
hydrotest of  low allo cladded coke drums to reduce cycle time.

Coke drum size :- 10 M OD X 45 M overall length. As per specification/
contract they have to do hydrotest.

Please share experts your suggestions for acceptance or rejection.


Regards,
Sachin A Kavathekar

NOTICE - This communication may contain confidential and privileged information that is for the sole use of the intended recipient. Any viewing, copying or distribution of, or reliance on this message by unintended recipients is strictly prohibited. If you have received this message in error, please notify us immediately by replying to the message and deleting it from your computer.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...