Wednesday, September 29, 2010

[MW:7281] RE: 7274] Re: pwht vs hardness

Hello Sunil/N.Patel

 

I am not sure whose query is this? As pointed out by Mr Bathula PWHT is mandatory for SA 672 Cl22 steel of 22 mm thickness. Your query does not specify the grade, however I‘m assuming that the material of construction is C.S and for 22 mm thk welds designed to B-31.3, PWHT is mandatory.

 

You need to speak to your welding engineer and give your constructions guys a back to basics course on welding, including hardness testing. Results of hardness testing are not “reproducible”, every indentation would yield different readings.

 

In simple word, based on the engineering principles, Spot hardness testing  can never be a substitute for PWHT.

 

Thanks.

 

Pradip Goswami,P.Eng.

Welding & Metallurgical Engineer/Specialist

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net

 

 

-----Original Message-----

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Raghuram Bathula

Sent: Wednesday, September 29, 2010 12:40 PM

To: Materials & Welding

Subject: [MW:7274] Re: pwht vs hardness

 

PWHT is mandatory by code for that thickness.

 

On Sep 29, 9:16 pm, "sunilrathor...@yahoo.com"

<sunilrathor...@yahoo.com> wrote:

 

> Dear member,

> 

> We have an pipe made from SA 672 cl 22 mat having dia 72" and thk 22 mm used for flair line in refinery. The construction people are taking deviation not to do pwht on basis that they will check the hardness value if it comes under limits they will not do pwht.

> 

> i want to know that is hardness testing is substitute for avoiding sr or pwht

> .

> Its design base is asme 31.3

> n Patel

 Worley Parsons, London

 

--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 


THIS MESSAGE IS ONLY INTENDED FOR THE USE OF THE INTENDED RECIPIENT(S) AND MAY CONTAIN INFORMATION THAT IS PRIVILEGED, PROPRIETARY AND/OR CONFIDENTIAL. If you are not the intended recipient, you are hereby notified that any review, retransmission, dissemination, distribution, copying, conversion to hard copy or other use of this communication is strictly prohibited. If you are not the intended recipient and have received this message in error, please notify me by return e-mail and delete this message from your system. Ontario Power Generation Inc.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...