[MW:7250] Using WPS qualified as per D1.1 to weld pipework as per ASME IX

Hello gents,

 I have a WPS qualified as per D1.1 – 8 inches for welding structural work, in 6G position,

My query is can I use these procedure to weld pipe work as per ASME IX for the same material?

Pls I need further clarification with codes support.

 

Regards

Philip Taiye

 

 


*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...