Hi Waqas,
                Go to Sec ix Article 3 & 2 , The welder Qualification Test report should represent the concern WPS For that project with Relevant PQR of that company only. If you are taking welders of diferent company in hire You have to Qualify them with your WPS ( perform wqt for new welders).
                So, you cannot use the Welder of other company. And you cannot submit any WPS OR PQR of different company. But if u give subcontracting to other company then you can qualify that welder with that WPS.
 
Regards.
Y.C.Shiva,
QA/QC Mech Engg,
Doha Qatar,
+974- 6166465. 

On Tue, Sep 15, 2009 at 10:19 PM, waqas suleman <waqas.suleman@gmail.com> wrote:
I have one query regarding the submition of WPS to client.In the starting of project i submitted a WPS for SMAW and GTAW for our project job.
Now i hired some welder from other company,but their certificate is certified on different WPS no.
Can i submit two WPS for the same job?bcause our PID inspecter rejected them for the approval of JCC card.
Please give me some refernce of code so i can convince them that they are applicable for this job.
 
 
Regards,
Waqas




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...