Wednesday, September 16, 2009

[MW:3231] Re: Two WPS for same Material and job

Hi!
Please refere QW-300.3 ASME sec IX, QW-301.2.
tHANKS & rEGARDS,
Vipin

On Tue, Sep 15, 2009 at 11:19 PM, waqas suleman <waqas.suleman@gmail.com> wrote:
I have one query regarding the submition of WPS to client.In the starting of project i submitted a WPS for SMAW and GTAW for our project job.
Now i hired some welder from other company,but their certificate is certified on different WPS no.
Can i submit two WPS for the same job?bcause our PID inspecter rejected them for the approval of JCC card.
Please give me some refernce of code so i can convince them that they are applicable for this job.
 
 
Regards,
Waqas




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...