[MW:3222] Re: Two WPS for same Material and job

Hello Wagas,

You have to qualify the hired welder as per the approved WPS (which
was submitted by you in the beginning); No codes permit you to proceed
as is...


Thanks
Senthil


On Sep 16, 12:19 am, waqas suleman <waqas.sule...@gmail.com> wrote:
> I have one query regarding the submition of WPS to client.In the starting of
> project i submitted a WPS for SMAW and GTAW for our project job.
> Now i hired some welder from other company,but their certificate is
> certified on different WPS no.
> Can i submit two WPS for the same job?bcause our PID inspecter rejected them
> for the approval of JCC card.
> Please give me some refernce of code so i can convince them that they are
> applicable for this job.
>
> Regards,
> Waqas

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...