Monday, September 14, 2009

[MW:3202] Re: DFT for paint

Please refer EN 10244 Part 5. 3 times higher than the nominal DFT on plus side.
regards,
rutvik

--- On Mon, 14/9/09, Tan Bui <tan281273@gmail.com> wrote:

> From: Tan Bui <tan281273@gmail.com>
> Subject: [MW:3194] DFT for paint
> To: "Materials & Welding" <materials-welding@googlegroups.com>
> Date: Monday, 14 September, 2009, 9:23 AM
>
> Dear all
> Can anyone show me about tolerance for DFT of paint fore
> Stacks system
> of power plant?
>
> Thanks in advance.
>
> Bui Van Tan
>
> >
>


See the Web's breaking stories, chosen by people like you. Check out Yahoo! Buzz. http://in.buzz.yahoo.com/

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...