Dear Mr Prabhakar,

U can use GTAW/SMAW/FCAW any one this is up to u and your repair
procedure.In your repaire procedure for SS material what welding
proceceses you have mentioned that all process u can use.

On Sep 9, 2:16 pm, Harikumar Dayalan / ZS Saudi PED QA/QC
<hariku...@zamilsteel.com> wrote:
> Dear friend
>
> Yes, you can use GTAW WPS for Fillet Repairs only.
>
> Where as for Groove repair welding, your WPS as to be qualified for QW -
> 451.2
>
> In case of Fillet repair weld, as per QW - 451.4 your WPS is applicable
> to weld All fillet size.
>
> Regards
>
> Harikumar Dayalan
>
> <mailto:hariku...@zamilsteel.com>  
>
>   _____  
>
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of prabhakar s
> Sent: Wednesday, September 09, 2009 11:41 AM
> To: materials-welding@googlegroups.com
> Subject: [MW:3150] Repair Weld
>
> Hi,
>
> We have to repair a fillet weld joint which is welded by SMAW process.
> Material is SS (A312 Gr316L). Can we do the repair with GTAW? Is it
> allowed as per any code? Please give me the reference also.
>
> We have a WPS for GTAW process on SS Material (A312 Gr316L).  
>
> Regards
>
> Prabhakar. S
>
> ---------------------------------------------------------------------------­-----------------------------
> Disclaimer: This email and any files transmitted with it are confidential
> and intended solely for the use of the addressee(s) named herein. If you
> are not the intended recipient or addressee, you should not use, disseminate,
> distribute, copy or alter this email. Any views or opinions presented in this
> email are solely those of the author and might not represent those of "Zamil
> Industrial" and or its units.
>
> Warning: Although reasonable precautions have been taken to ensure no viruses
> are present in this email, the company cannot accept responsibility for any
> loss or damage arising from the use of this email or attachments. If you have
> received this electronic mail message in error, please contact the sender directly.

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...