Hi!Guys we have a new job in super duplex piping, i want to develpo a
wps for the base material as listed below.

A815, A 928 & SA 182 F53. Could you please suggest whether i can
qualify S,No 10 H Gr 1 material from the PQR i run for P.No 10 H Gr 1
material .Also it would be helpful if any one can provide a sample
wps.
Please Revert.
Thanks & Regards,
vipin

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...