[MW:3134] RE: 3133] Weld over lay on the inner surface of an elbow

Assuming your design code as B31.3 for ¾” wall thickness no PWHT is required for the weld overlay, since it is not a metal to metal contact, any Stainless steel weld overlay can serve the purpose.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Chandulal Vithlani
Sent: Tuesday, September 08, 2009 9:33 AM
To: materials-welding@googlegroups.com
Subject: [MW:3133] Weld over lay on the inner surface of an elbow

 

We have a problem of erosion by steam + water jet.

 

Material of the elbow is A234-WPBW Thickness: 0.75” Diameter: 28” Long Radius

 

We would like to have hard facing on the inner surface without the need for PWHT.

 

Can any one suggest suitable WPS for the same?

 

Regards

 

Chandulal S Vithlani

 

 

 



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...